<?xml version="1.0" encoding="utf-8"?>
|
|
<CutterMaterial>
|
|
<Name>WC-Co6-500nm-Advanced</Name>
|
|
<Note>Advanced tungsten carbide with 6% cobalt binder, 500nm grain size, and optimized properties</Note>
|
|
<ElasticModulus_GPa>640</ElasticModulus_GPa>
|
|
<TensileStrength_MPa>1580</TensileStrength_MPa>
|
|
<ThermalExpansionCoefficient_dMK>6.4</ThermalExpansionCoefficient_dMK>
|
|
<HeatConductivity_WdmK>98</HeatConductivity_WdmK>
|
|
<HeatCapacity_JdgK>0.28</HeatCapacity_JdgK>
|
|
<Density_gdcm3>15.1</Density_gdcm3>
|
|
<PoissonRatio>0.21</PoissonRatio>
|
|
<MeltingTemperature_K>3173</MeltingTemperature_K>
|
|
<FusionLatentHeat_Jdg>420</FusionLatentHeat_Jdg>
|
|
<FrictionCoefficient>0.38</FrictionCoefficient>
|
|
<TemperatureVsHardnessCurve>
|
|
<Entry Temperature_K="298">18700</Entry>
|
|
<Entry Temperature_K="873">16200</Entry>
|
|
<Entry Temperature_K="1013">14100</Entry>
|
|
<Entry Temperature_K="1173">11800</Entry>
|
|
<Entry Temperature_K="1273">11800</Entry>
|
|
<Entry Temperature_K="1373">11800</Entry>
|
|
<Entry Temperature_K="1473">11800</Entry>
|
|
</TemperatureVsHardnessCurve>
|
|
<TemperatureVsWearCoefficientCurve>
|
|
<Entry Temperature_K="298">0.92</Entry>
|
|
<Entry Temperature_K="473">1.45</Entry>
|
|
<Entry Temperature_K="673">5.80</Entry>
|
|
<Entry Temperature_K="873">19.40</Entry>
|
|
<Entry Temperature_K="973">32.60</Entry>
|
|
<Entry Temperature_K="1073">51.80</Entry>
|
|
<Entry Temperature_K="1173">74.50</Entry>
|
|
<Entry Temperature_K="1273">105.00</Entry>
|
|
<Entry Temperature_K="1373">145.00</Entry>
|
|
<Entry Temperature_K="1473">195.00</Entry>
|
|
</TemperatureVsWearCoefficientCurve>
|
|
</CutterMaterial>
|