2025-07-18 15:38:28 +08:00

37 lines
1.6 KiB
XML

<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>WC-Co10-600nm</Name>
<Note>Tungsten carbide with 10% cobalt binder and 600nm grain size, offering improved toughness for interrupted cutting</Note>
<ElasticModulus_GPa>580</ElasticModulus_GPa>
<TensileStrength_MPa>1680</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>7.1</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>85</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.27</HeatCapacity_JdgK>
<Density_gdcm3>14.5</Density_gdcm3>
<PoissonRatio>0.23</PoissonRatio>
<MeltingTemperature_K>3123</MeltingTemperature_K>
<FusionLatentHeat_Jdg>390</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.42</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">16200</Entry>
<Entry Temperature_K="873">13600</Entry>
<Entry Temperature_K="1013">11400</Entry>
<Entry Temperature_K="1173">9200</Entry>
<Entry Temperature_K="1273">9200</Entry>
<Entry Temperature_K="1373">9200</Entry>
<Entry Temperature_K="1473">9200</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">1.35</Entry>
<Entry Temperature_K="473">2.10</Entry>
<Entry Temperature_K="673">7.80</Entry>
<Entry Temperature_K="873">28.40</Entry>
<Entry Temperature_K="973">46.70</Entry>
<Entry Temperature_K="1073">74.20</Entry>
<Entry Temperature_K="1173">103.50</Entry>
<Entry Temperature_K="1273">142.00</Entry>
<Entry Temperature_K="1373">190.50</Entry>
<Entry Temperature_K="1473">250.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>